In the PCBA processing process, due to process or manual factors, a small amount of tin balls and dross may be left on the PCBA board. The tin beads and tin dross will loosen in an uncertain environment, forming a short circuit of the PCBA board, and finally causing the product to fail.

The following are some measures to reduce PCBA tin beads and dross:

 1. Pay attention to the production of stencil. It is necessary to adjust the size of the opening appropriately in combination with the specific component layout of the PCBA board to control the printing volume of solder paste. Especially for some dense foot components or board surface components are denser.

 2. For PCB bare boards with BGA, QFN and dense-foot components on the board, strict baking action is recommended to ensure that moisture on the pad surface is removed, to maximize solder ability and prevent the generation of tin beads

 3. Inn hand soldering workrooms, clean the countertop in time, and strengthen the visual inspection of the SMD components around the manually soldered components, focus on checking whether the solder joints of the SMD components are accidentally touched and dissolved or the tin balls and dross are scattered among the component pins.