The "tombstone" phenomenon often occurs in the reflow soldering process of CHIP components (such as chip capacitors and chip resistors). The smaller the component, the more likely it is. So how to avoid this kind of problem as much as possible? The following are several points of attention for pad design, placement position, and solder paste thickness:
(1) Design the pads reasonably. The use of different pad sizes may cause unbalanced pad heating and solder paste flow time. The extension size of the pad must be reasonable, and try to avoid the situation where the wetting angle of the outer edge (straight line) of the pad formed by the extension length is greater than 45°.
(2) Strictly control the quality of materials to ensure that the effective areas of the two ends of the components used are the same. In order to ensure that when the solder paste melts, the resultant force acting on the solder joints on the component is zero, so as to facilitate the formation of ideal solder joints.
(3) The placement of the patch must be accurate. Avoid large patch deviations that can lead to component tombstone phenomenon.
(4) Reduce the thickness of the solder paste, and reduce the heating rate during reflow soldering. When the thickness of the solder paste becomes smaller, the tombstone phenomenon will be greatly reduced. The solder paste becomes thinner, the heat capacity of the entire pad is reduced, and the probability of the solder paste on the two pads being melted at the same time is greatly increased.